this is the view of first coil only 1 wrap around, as I found out it doesn't matter how many coils you use for air.
This is how i fluidized casting sand, I used the finest and blasting sand I could get from our local concrete supply outfit and they also carry bentonite, fireclay and vulcanic perlite. The sand was mixed to about 10% bentinite clay.